Powder Coating procedures for external and internal structural components.

Inspect the product for flaws or defects, repair as needed

Sandblasting product (galvanized or bare steel) 0.75 - 1.5 mil. Profile compatible with SSPC-SP-10 (NACE 2 - near white metal scraper) for bare steel, SSPC-SP-7 (NACE 4 - Brushing scraper) for galvanized steel.

Preheat the oven to 450 ° F.

Mask teeth, machined surfaces and anything else that's needed.

Clean the product with compressed air.

Put the product in the oven for pre-cooking.

Pre-cook the product at 450 F. Verify product temperature is 375 F on the entire product before applying primer.

Take the product out of the oven and apply 2.5 - 3.5 mil. Zinc rich epoxy primer in powder base produces specifications on hot product so it melts on contact.

Allow the product to cool between 125 ° F and 175 ° F

Apply 2.5 - 3.5 mil. It produces top coat according to powder production properties.

Place the product in the oven at 425 ° - 435 ° F until the entire substrate falls within the curing window indicated by the powder manufacturer.

Remove from oven to cool, check, de-mask and drain.

Wrap and pack the product.